Scattered glaze pits, moderate surface wear and scattered scratches; filled TL test holes to footring; under Uv light, no additional repairs or restorations seen. According to a copy of an Oxford Authentication thermoluminescence analysis report No.: P108g75, dated 11 March, 2008, the results were consistent with the proposed dating of this object (report no longer present). 據牛津實驗室2008年3月11日熱釋光鋻定報告,編號P108g75,鑒定到代。